Freeze and Fuse with UGC Layering Mix
sue darte
0:00 / 0:00
Freeze and Fuse with UGC Layering Mix
36 849 просмотров · 4 года назад
sue darte
925 подписчиков
36 849 просмотров · 4 года назад
Demonstration on using UGC Layering Mix with powdered frit for making freeze & fuse glass.
Here are a few places where you can purchase UGC Layering Mix.
My schedule was as follows, but again, that's my kiln and maybe too conservative, due to lack of experience. COE96
It smells, so you want to vent to 800
400/1320/15
9999/950/60
300/100/0
Note: In addition to using colored frit, I have also tested with clear frit and then after firing, I have painted with enamel paint and put back into the kiln to fuse the paint to the glass (sintering)
350/1385/20
9999/950/30
100/700/0
one last note: I've also tested with the sludge that comes from my grinder. Scraped it up, sifted it and used it to make freeze and fuse pieces
Unique Glass Colors
https://www.uniqueglasscolors.com/
Colors for Earth
https://colorsforearth.com
Anything In Stained Glass
https://www.anythinginstainedglass.co...
If you have questions, you can reach me at info@darteglass.com